GTAW rod for analogous, heat resisting, rolled, forged and cast steels, e.g. in annealing shops, hardening shops, steam boiler construction, the crude oil industry and the ceramics industry.
Read more
- Fully austenitic deposit. Preferably employed for applications involving the attack of oxidizing, nitrogencontaining or low-oxygen gases. - The final layer of joint welds in heat resisting CrSiAl steels exposed to sulphurous gases must be deposited by means of FOX FA or FA-IG. - Scaling resistance up +1200 °C. Cryogenic toughness down to –196 °C. - The temperature range between +650 °C and 900°C should be avoided owing to the risk of embrittlement. - Yield strength: 420 MPa - Tensile strength: 630 MPa - Elongation: 33 % |
Thermanit 310 MN 2,4x1000mm
Böhler 81030 (5kg)
Product number: 10120013278
Wholesale lot 20 kg
Sold in full packages. For smaller quantities, contact your nearest Megacenter store.
Details
Technical details
| Sales unit | Kilogram |
|---|---|
| Halkaisija -ø mm | 2,4 |